Kopsavilkums
P92 heat-resistant steel has been successfully submerged arc welded by employing designed CaF2–Cr2O3 fluxes. It has been demonstrated that δ-ferrite is retained in the weld metal, the area fraction of which is found an approximately 3.7-fold enhancement as the Cr2O3 content in the fluxes is raised from 5 to 25 wt pct. Such phenomenon has been elucidated through governing element transfer behaviors incurred by the decomposition of Cr2O3. Our findings possibly offer a viable solution towards developing welding fluxes geared towards durable heat-resistant steel grades.
| Oriģinālvaloda | Angļu |
|---|---|
| Lapas (no-līdz) | 2169-2174 |
| Žurnāls | Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science |
| Sējums | 55 |
| Izdevuma numurs | 7 |
| DOIs | |
| Publikācijas statuss | Publicēts - jūl. 2024 |
OECD Zinātnes nozare
- 1.3 Fizika un astronomija
Nospiedums
Uzziniet vairāk par pētniecības tēmām “δ-Ferrite Retention in the Weld Metal of P92 Heat-Resistant Steel Treated by CaF2–Cr2O3 Fluxes”. Kopā tie veido unikālu nospiedumu.Citēt šo
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver