From the dielectric measurements of the relaxor ceramics BaBi 2Ta2O9 (BBT) in a wide frequency range (10 1-1011 Hz) the real distribution function of the relaxation times f(τ) was calculated. The shape of the distribution function is asymmetrical in all measured temperature interval with the expressed peak of relaxation times about 10-12s in higher temperatures.