Kopsavilkums
Na-Al-Si glass fabrics fibres contain Na+ ions that diffuse to its surface and along with CO2 and H2O from atmosphere create here the shell of carbonate hydrates. The heating of fabric leads to weight loss by evolving these substances. In this work the results of weight recovery study at room relative humidity (20%-50%) and elevated humidity (near 70%) of fabrics after its heating at different temperatures (70°C-150°C) are compared. The experiments shoved the different weight recovery kinetics. The initial exponential stages up to 0.3 h-0.5 h of the both recoveries are associated with water absorption and differ by its levels. In a case of lower environment humidity the later weight increase are restricted by its value, but at an elevated humidity has a maximum and followed weight increase. The reasons of observed differences are discussed.
| Oriģinālvaloda | Angļu |
|---|---|
| Raksta numurs | 012021 |
| Žurnāls | IOP Conference Series: Materials Science and Engineering |
| Sējums | 77 |
| Izdevuma numurs | 1 |
| DOIs | |
| Publikācijas statuss | Publicēts - 2015 |
| Pasākums | 12th Russia/CIS/Baltic/Japan Symposium on Ferroelectricity, RCBJSF 2014 and 9th International Conference on Functional Materials and Nanotechnologies, FM and NT 2014 - Riga, Latvija Ilgums: 29 sept. 2014 → 2 okt. 2014 |
OECD Zinātnes nozare
- 1.3 Fizika un astronomija
Nospiedums
Uzziniet vairāk par pētniecības tēmām “Environment humidity effect on the weight of carbonized Na-Al-Si glass fabrics recovery after heating”. Kopā tie veido unikālu nospiedumu.Citēt šo
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver