Pāriet uz galveno navigāciju Pāriet uz meklēšanu Pāriet uz galveno saturu

Ferroelectric and ferromagnetic properties of Gd-doped BiFeO3-BaTiO3 solid solution

  • Radheshyam Rai*
  • , Igor Bdikin
  • , Manuel Almeida Valente
  • , Andrei L. Kholkin
  • *Šī darba korespondējošais autors
  • University of Aveiro

Zinātniskās darbības rezultāts: Devums žurnālamZinātniskais raksts (žurnālā)koleģiāli recenzēts

67 Atsauces (Scopus)

Kopsavilkums

The solid solutions of Bi1-x-yGdxBayFe1-yTi yO3 have been prepared via solid-state reaction method with the aim to obtain magnetoelectric coupling (i.e., linear relation between magnetization and electric field) at room temperature. Optimum calcination and sintering strategies for obtaining pure perovskite phase, high density ceramics and homogeneous microstructures have been determined. All the samples of the composition Bi1-x-yGdxBayFe1-yTi yO3 (x = 0.1 and y = 0.1, 0.2, and 0.3) reported in the present work are tetragonal at room temperature. The maximum ferroelectric transition temperature (Tc) of this system was 150-170 °C with the dielectric constant peak of 2300 at 100 kHz for y = 0.1. Above Tc the dielectric constant is decreasing up to a certain temperature and then increasing with temperature similar to that observed in other perovskites due to chemical inhomogeneities in both A and B sites of the ABO3 cell. The variation of ferroelectric and magnetic properties was followed by piezoresponse force microscopy and vibrating sample magnetometer, respectively. Well-saturated piezoelectric loops were observed for all composition indicating room temperature ferroelectricity.

OriģinālvalodaAngļu
Lapas (no-līdz)539-545
Lapu skaits7
ŽurnālsMaterials Chemistry and Physics
Sējums119
Izdevuma numurs3
DOIs
Publikācijas statussPublicēts - 15 febr. 2010
Ārēji publicēts

Nospiedums

Uzziniet vairāk par pētniecības tēmām “Ferroelectric and ferromagnetic properties of Gd-doped BiFeO3-BaTiO3 solid solution”. Kopā tie veido unikālu nospiedumu.

Citēt šo