Kopsavilkums
Mixed Ta-Re oxide thin films were synthesised for the first time by dc magnetron co-sputtering. Local environment around tantalum and rhenium atoms was studied by the Ta and Re L3-edges x-ray absorption spectroscopy in pure Ta2O5 and mixed Ta-Re oxide thin films (Ta:Re= 50:50, 38:62, 20:80 as determined from the ratio of the Ta-to-Re absorption edges). It was found that rhenium atoms are four-fold coordinated by oxygen atoms with R(Re-O)=1.74±0.01 Å and the mean square relative displacement (MSRD) σ2=0.0012±0.0005 Å 2. In pure Ta2O5 thin film, tantalum ions are coordinated by six oxygen atoms at R(Ta-O)=2.02±0.01 Å with the MSRD σ20.010±0.0001 Å2. The addition of rhenium ions shortens the Ta-O distance by about 0.02-0.03 Å and makes the Ta-O distances distribution slightly broader with the MSRD σ 2≈0.013±0.001 Å2. The high frequency contribution in the Ta L3-edge EXAFS signals, which is responsible in its Fourier transform for the peak beyond the first coordination shell, is due to the multiple-scattering effects within distorted [TaO6] octahedron.
| Oriģinālvaloda | Angļu |
|---|---|
| Lapas (no-līdz) | 79-85 |
| Lapu skaits | 7 |
| Žurnāls | Proceedings of SPIE - The International Society for Optical Engineering |
| Sējums | 5122 |
| DOIs | |
| Publikācijas statuss | Publicēts - 2002 |
| Pasākums | PROCEEDINGS OF SPIE SPIE - The International Society for Optical Engineering: Advanced Organic and Inorganic Optical Materials - Riga, Latvija Ilgums: 19 aug. 2002 → 22 aug. 2002 |
Nospiedums
Uzziniet vairāk par pētniecības tēmām “Local structure of Ta-Re mixed oxide thin films studied by x-ray absorption spectroscopy”. Kopā tie veido unikālu nospiedumu.Citēt šo
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver